Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrason® S 3010 NAT - PSU - BASF

Material Data Center offers the following functions for Ultrason® S 3010 NAT:
unit conversion, PDF datasheet print, comparison with other plastics, parameters for material models, CAE Interfaces

Check here, which other Ultrason S datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Unreinforced, higher viscosity injection moulding and extrusion grade, tougher and with improved chemical resistance.
Abbreviated designation according to ISO 1043-1: PSU
Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 55 / * cm³/10min ISO 1133
Température 360 / * °C -
Charge 10 / * kg -
Retrait au moulage, parallèle 0.7 / * % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 0.7 / * % ISO 294-4, 2577
Température d'éjection 165 °C -
ASTM Data
Retrait au moulage , parallèle 0.007 mm/mm ASTM D 955
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction - / 2550 MPa ISO 527
Contrainte d'écoulement - / 75 MPa ISO 527
Déformation au seuil d'écoulement - / 5.5 % ISO 527
Déformation nominale à la rupture - / >50 % ISO 527
Module de fluage en traction, 1h * / 2500 MPa ISO 899-1
Résistance au choc Charpy, +23°C - / N kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C - / N kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C - / 5.5 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C * / 6 kJ/m² ISO 179/1eA
ASTM Data
Module de traction d’élasticité 80 / - MPa ASTM D 638
Allongement d’élasticité 5.7 / - % ASTM D 638
Module de flexion 2599 / - MPa ASTM D 790
Izod choc avec entaille, 1/8 in 10 / - J/m ASTM D 256
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de transition vitreuse, 10°C/min 187 / * °C ISO 11357-1/-2
Température de fléchissement s/chrg, 1.80 MPa 176 / * °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 183 / * °C ISO 75-1/-2
Température de ramolliss. Vicat, B 183 / * °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 53 / * E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm HB / * class IEC 60695-11-10
Epaisseur de l'éprouvette 1.6 / * mm -
Yellow Card disponible oui / * - -
Inflammabilité pr. épaisseur h V-2 / * class IEC 60695-11-10
Epaisseur de l'éprouvette 3.0 / * mm -
Yellow Card disponible oui / * - -
Aptitude à l'allumage 32.1 / * % ISO 4589-1/-2
ASTM Data
DTUL à 66 psi 182 °C ASTM D 648
DTUL à 264 psi 171 °C ASTM D 648
Propriétés électriquessec / condUnitéNorme du test
ISO Data
Permittivité relative, 100Hz * / 3.1 - IEC 62631-2-1
Permittivité relative, 1MHz * / 3.1 - IEC 62631-2-1
Facteur de pertes, 100Hz * / 8 E-4 IEC 62631-2-1
Facteur de pertes, 1MHz * / 64 E-4 IEC 62631-2-1
Résistivité transversale * / >1E13 Ohm*m IEC 62631-3-1
Résistivité superficielle * / >1E15 Ohm IEC 62631-3-2
Rigidité diélectrique * / 37 kV/mm IEC 60243-1
Indice de résistance au cheminement * / 125 - IEC 60112
Propriétés diversessec / condUnitéNorme du test
Absorption d'eau 0.8 / * % Sim. to ISO 62
Absorption d'humidité 0.3 / * % Sim. to ISO 62
Masse volumique 1230 / - kg/m³ ISO 1183
Densité 1240 kg/m³ ASTM D 792
Propriétés spécifiques à la matièresec / condUnitéNorme du test
ISO Data
Indice de viscosité 72 / * cm³/g ISO 307, 1157, 1628
Préparation et conditionnement des éprouvettesValeurUnitéNorme du test
ISO Data
Injection, température de la matière fondue 360 °C ISO 294
Injection, température du moule 140 °C ISO 294
Injection, vitesse d'injection 200 mm/s ISO 294
Injection, pression de maintien 70 MPa ISO 294
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 140 °C -
Pré-séchage - temps 4 h -
L'humidité de traitement ≤0.02 % -
Température de la matière fondue 330 - 390 °C -
Température du moule 120 - 160 °C -
Fonctions
Viscosité / Vitesse de cisaillement , Ultrason® S 3010 NAT, PSU, BASF
Contrainte de cisaillement / Vit. de cisaillement , Ultrason® S 3010 NAT, PSU, BASF
Contrainte / Déformation , Ultrason® S 3010 NAT (cond.), PSU, BASF
Module sécant / Déformation , Ultrason® S 3010 NAT (cond.), PSU, BASF
Contrainte / Déformation (isochrone) 23°C, Ultrason® S 3010 NAT (cond.), PSU, BASF
Module de fluage / Temps 23°C, Ultrason® S 3010 NAT (cond.), PSU, BASF
Courbe de fluage 23°C, Ultrason® S 3010 NAT (cond.), PSU, BASF
Volume spécifique (pvT) , Ultrason® S 3010 NAT, PSU, BASF
Module de traction / Température , Ultrason® S 3010 NAT (cond.), PSU, BASF
Fatigue strength , Ultrason® S 3010 NAT, PSU, BASF
Caractéristiques
Transformation
Moulage par injection, Extrusion de films, Extrusion de profilés, Extrusion de plaques, Soufflage, Thermoformage
Conditionnement
Granulés, Couleurs naturelles
Disponibilité régionale
Autres informations
Moulages par injection
PREPROCESSING
Pre/Post-processing, max. allowed water content: .02 %
Pre/Post-processing, Pre-drying, Temperature: 140 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 330 - 390 °C
injection molding, Melt temperature, recommended: 350 °C
injection molding, Mold temperature, range: 120 - 160 °C
injection molding, Mold temperature, recommended: 140 °C
injection molding, Dwell time, thermoplastics: 10 min

Pretreatment
Drying temperature: 130 - 150°C
Drying time: minimum 4h
recommended dryer: vaccum or dry air dryer
maximum moisture: 0,02 - 0,05%

Ultrason® can be injection molded by any type of machinery on the market, provided that the plasticizing unit and the mold temperature control system have been configured appropriately. The machinery manufacturer must be consulted if any doubts exist on the ability of various parts to withstand the high temperatures required (e.g. barrel, barrel head, bolted connections, etc.)

Long residence time in combination with high temperatures should be avoided e.g. by pump out material at regular intervals.
During extended interruptions, the barrel temperature should be lowered to about 250-280°C.

It has been found out that heating to the requested processing temperature and shutting down or lowering the temperature is best carried out in two steps.
First, the barrel temperatures are set at the lower processing temperature range for the particular thermoplastic (340 - 350 °C). As soon as these temperatures have reached a steady state, the material in the barrel is pumped out. Second, the barrel temperature can be set to the required processing temperature or the heaters can be shut down.
Résistance Chimique
Acides
Acide acétique (masse en 5%) (23°C)
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com